Dit platform verschaft informatie en kennis omtrent de WL expertisedomeinen 'hydraulica en sediment', 'havens en waterwegen', 'waterbouwkundige constructies', 'waterbeheer' en 'kustbescherming' - gaande van WL medewerkers met hun expertise, het curriculum van deze instelling, tot publicaties, projecten, data (op termijn) en evenementen waarin het WL betrokken is.
Het WL onderschrijft het belang van "open access" voor de ontsluiting van haar onderzoeksresultaten. Lees er meer over in ons openaccessbeleid.
one publication added to basket [223753] |
Synthesized mercaptopropyl nanoporous resins in DGT probes for determining dissolved mercury concentrations
Gao, Y.; De Canck, E.; Leermakers, M.; Baeyens, W.; Van Der Voort, P. (2011). Synthesized mercaptopropyl nanoporous resins in DGT probes for determining dissolved mercury concentrations. Talanta 87: 262-267. http://dx.doi.org/10.1016/j.talanta.2011.10.012
In: Talanta. Elsevier: Amsterdam. ISSN 0039-9140; e-ISSN 1873-3573
| |
Trefwoord |
|
Author keywords |
Diffusive Gradients in Thin films; Labile Hg; SH-SBA; SH-PMO; SQR; SH-KG |
Auteurs | | Top |
- Gao, Y.
- De Canck, E.
- Leermakers, M.
|
- Baeyens, W.
- Van Der Voort, P.
|
|
Abstract |
3-Mercaptopropyl functionalized SBA-15 (SH-SBA) and 3-mercaptopropyl functionalized ethenylene bridged periodic mesoporous organosilica (SH-PMO) were included in a Diffusive Gradients in Thin film (DGT) probe and compared to similar commercially available resins also containing thiol functional groups, such as Sumichelate Q10R (SQR) and 3-mercaptopropyl functionalized silica gel (SH-KG), and also to the Chelex-100 resin for the determination of labile Hg concentrations. An agarose gel was used as the diffusive gel because the classic polyacrylamide gel shows more than 20% of Hg adsorption. According to our results, the Chelex-100 resin presents a much lower affinity for Hg than the thiol based resins. The non-linear accumulation profile of mercury with time for the Chelex-100 resin makes it in fact impossible to use Fick's law for estimating the diffusion coefficient of Hg. The 4 other resins all show a linear accumulation profile of Hg with time. Although the highest accumulation rate is observed for SH-PMO followed by SQR, SH-SBA and SH-KG, these values do not differ very much. |